Stresses in electron beam weld joints of superalloys. (News Briefs).


Single crystalline turbine blades are the pinnacle of a decade-long development and refinement of nickel-based superalloys. Because of the considerable investment in manufacturing, electron beam welding Electron beam welding (EBW) is a fusion welding process in which a beam of high-velocity electrons is applied to the materials being joined. The workpieces melt as the kinetic energy of the electrons is transformed into heat upon impact, and the filler metal, if used, also melts to  with a polycrystalline Adj. 1. polycrystalline - composed of aggregates of crystals; "polycrystalline metals"
crystalline - consisting of or containing or of the nature of crystals; "granite is crystalline"
 replacement material is used to repair minor structural damage of failed components of these otherwise poorly weldable materials. While both the fusion zone and the heat affected zone are small, about one millimeter, the cooling rates are high so that very high residual stresses Residual stresses are stresses that remain after the original cause of the stresses (external forces, heat gradient) has been removed. They remain along a cross section of the component, even without the external cause.  are generated.

In order to study the efficiency of stress relief, scientists from the NIST (National Institute of Standards & Technology, Washington, DC, www.nist.gov) The standards-defining agency of the U.S. government, formerly the National Bureau of Standards. It is one of three agencies that fall under the Technology Administration (www.technology.  Center for Neutron Research and a private company have investigated by means of neutron diffraction Neutron diffraction

The phenomenon associated with the interference processes which occur when neutrons are scattered by the atoms within solids, liquids, and gases.
 the residual stress distribution both in the as-welded state and after a heat treatment. The heat treatment includes a solution treatment and subsequent aging. The typical grain size of the polycrystal side of the weld joint was approximately one millimeter which is about the size of the incident neutron beam. Thus, stress measurements could be done only on the single crystal side of the joint.

It was found that the as-welded sample exhibits tensile stresses tensile stress

See under axial stress.
 on the order of the yield stress both parallel and perpendicular to the weld. We have also found evidence for solution partitioning and a substantial level of plastic strain both in the fusion zone and in an approximately half-millimeter wide heat affected zone. Both effects are completely removed after the heat treatment. The heat treatment also removes very effectively and completely the detrimental tensile residual stresses in the extended weld zone. These results are the first on this type of system, in which single-crystal and polycrystalline constituents are joined.

CONTACTS: Thomas Gnaupel-Herold, (301) 975-5380; thomas.gnaeupel-herold@nist.gov or Henry Prask, (301) 975-6226; henry.prask@nist.gov.
COPYRIGHT 2002 National Institute of Standards and Technology
No portion of this article can be reproduced without the express written permission from the copyright holder.
Copyright 2002, Gale Group. All rights reserved. Gale Group is a Thomson Corporation Company.

 Reader Opinion

Title:

Comment:



 

Article Details
Printer friendly Cite/link Email Feedback
Publication:Journal of Research of the National Institute of Standards and Technology
Article Type:Brief Article
Geographic Code:1USA
Date:Jan 1, 2002
Words:285
Previous Article:NIST AIDS development of new bone graft materials. (News Briefs).(Brief Article)
Next Article:Patient issued for reverse-angle X-ray diffraction. (News Briefs).(Brief Article)
Topics:



Related Articles
Firing long-distance electrons.
Subatomic scrutiny from Jefferson lab.(improved picture of quarks produced at Thomas Jefferson National Accelerator Facility)(Brief Article)
CLINTON DEFENDERS FIRE BACK; IMPEACHMENT ACT CALLED `VENGEANCE'.(News)
AREA HOSPITAL SUES WELDING-METAL MAKER.(NEWS)
Investigate resistance of bacteria to E-beam technology.
Be aware of factors that affect antimicrobial action of electron beams.
Correction.(Correction Notice)
The disk difference: Improving laser output; It's smaller and provides a more powerful beam. It's based on Yb:YAG, so it can be deployed through an...
Fujitsu and Advantest to Establish Joint Venture to Create Semiconductor Prototypes Using Electron Beam Direct Lithography.

Terms of use | Copyright © 2009 Farlex, Inc. | Feedback | For webmasters | Submit articles