MDI for elastomers has lower freeze point.A carbodiimide-modified MDI (1) (Multiple Document Interface) A Windows function that allows an application to display and lets the user work with more than one document at the same time. reportedly features improved low-temperature stability, clarity, and shelf-life compared with similar PUR raw materials for elastomers. New Lupranate 5143 from BASF BASF Bar Association of San Francisco (since 1872; San Francisco, California) BASF Badische Anilin und Soda Fabrik (German chemical products company) BASF Builders Association of South Florida Corp., Urethanes Div., Wyandotte, Mich., is designed to produce soft elastomers with high elongation and HDT HDT Heat Deflection Temperature (plastics) HDT High Dose Therapy HDT Heatpipe Direct Touch (Xigmatek) HDT Heat Distortion Temperature (plastics) HDT Henry David Thoreau plus good impact, tear, and tensile strengths. It reportedly gives longer gel time than competing materials, and also has a lower freeze point than previous carbodiimide-modified MDIs, such as monomeric monomeric /mono·mer·ic/ (mon?o-mer´ik) 1. pertaining to, composed of, or affecting a single segment. 2. in genetics, determined by a gene or genes at a single locus. 4,4 MDI. Better low-temperature stability helps ease handling for field formulators. Tel: (800) BC-RESIN * PTDirect: 517FV |
|
||||||||||||||||

Printer friendly
Cite/link
Email
Feedback
Reader Opinion